Effect Of Preheating On The Hardness And Microstructure In Shielded Metal Arc Weldments Of A283 B

Main Article Content

Ali Akbar

Abstract

The purpose of this study was to determine the effect of heating on the welding process of SMAW (Shielded Metal Arc Welding) in terms of hardness and microstructure of welded metal. Much welding has been done by preheating but below the temperature used below the initial martensitic temperature which reaches 452 ° C, this data is sourced from research by S.Zheng et.al and Y. Huang et.al. For this reason, an experiment was carried out with heat temperatures above a martensitic temperature of 500 ° C. The results show that in the Weld Metal area the pearlite structure appears larger, the effect of current strength on HAZ width is directly proportional, the greater the current strength, the wider HAZ, and hardness are affected by the rough grains of martensite

Article Details

Section
Articles

References

[1] Buchely MF, Gutierrez JC, Leon LM, Toro A. The effect of microstructure on abrasive wear of hardfacing alloys. Wear 2005;259:52–61.
[2] Iswanto et al., Effect of Welding Using Electrodes With Certain Treatment on Stainless Steel 304 Using SMAW Welding, Covenant Journal of Engineering Technology, vol. 4, no. 2, pp. 50-55, 2020.
[3] Iswanto, Noerdianto, A’rasy Fachruddin dan Mulyadi, Analisa Perbandingan Kekuatan Hasil Pengelasan TIG dan Pengelasan MIG pada Aluminium 5083, Jurnal Turbo, vol. 9, no. 1, pp. 87-92, 2020.
DOI: http://dx.doi.org/10.24127/trb.v9i1.1166
[4] P.K. Ghosh, U. Singh, Influence of pre- and post-weld heating on weldability of modified 9Cr–1Mo(V–Nb) steel pipe under shielded metal arc and tungsten inert gas welding processes, Sci. Technol. Weld. Joining 9 (3) (2004) 229–236.
[5] P. Deb, K.D. Challenger, D.R. Clark, Transmission electron microscopy characterizations of preheated and non-preheated shielded metal arc weldments of HY-80 steel, Mater. Sci. Eng. 77 (1986) 155–167.
[6] J.O. Olawale, S.A. Ibitoye, K.M. Oluwasegun, M.D. Shittu, R.C. Ofoezie, Correlation between process variables in shielded metal arc welding (SMAW) process and post weld heat treatment (PWHT) on some mechanical properties of low carbon steel welds, J. Min. Mater. Charact. Eng. 11 (2012) 891–895.
[7] Abdullah Mohd Tahir, Noor Ajian Mohd Lair, Foo Jun Wei, Investigation on mechanical properties of welded material under different types of welding filler (Shielded Metal Arc Welding), in: AIP Conference Proceedings-3rd International Conference on the Science and Engineering of Materials (ICoSEM 2017), 2018.
[8] Aman Gupta, Amit Kumar, T. Baskaran, Shashi Bhushan Arya, Rajesh Kisni Khatirkar, Effect of heat input on microstructure and corrosion behaviour of duplex stainless-steel shielded metal arc welds, Trans. Indian Inst. Metals 77 (7) (2018) 1595–1606.
[9] Munawar, Hammada Abbas, Ahmad Yusran Aminy, The effects of shielded metal arc welding (smaw) welding on the mechanical characteristics with heating treatment in S45c steel, J. Phys.: Conf. Series 962 (1) (2018.
[10] Yu. Weiwei, Minyu Fan, Jinhua Shi, Xu. Fei Xue, Hui Liu Chen, A comparison between fracture toughness at different locations of SMAW and GTAW welded joints of primary coolant piping, Eng. Fract. Mech. 202 (2018) 135–146.
[11] Iswanto, Edi Widodo, Ali Akbar dan Angga Kharisma Putra, Perbandingan Induction Hardening dengan Flame Hardening pada Sifat Fisik Baja ST 60, Mekanika: Majalah Ilmiah Mekanika, vol. 19, no. 2, 2020.
DOI: https://doi.org/10.20961/mekanika.v19i2.43203
[12] H.K.D.H. Bhadeshia, R.W.K. Honeycombe, Steels Microstructure and Properties, Butterworth-Heinemann, 2011
[13] G. Thewlis, Classifcation and quantification of microstructures in steels, Mater. Sci. Technol. 20 (2004) 143–160.
[14] S. Zheng, Q. Wu, Q. Huang, et al., Influence of different cooling rates on the mi- crostructure of the HAZ and welding CCT diagram of CLAM steel, Fusion Eng. Des. 86 (2011) 2616–2619.
[15] Y. Huang, X. Chen, Z. Shen, et al., Measurement and analysis of SHCCT diagram for CLAM steel, J. Nucl. Mater. 432 (s1-3) (2013) 460–465.